Sink Marks in Injection Molded Appliance Parts: Causes and Checks

DAYIN 技術團隊2 分鐘閱讀
在辦公室的電腦工作站前工作的團隊成員

A sink mark is a depression on a molded surface. It often appears opposite a thick section, rib, boss or internal fillet where the material cools and contracts differently from the surrounding wall. A void is an internal cavity; the two defects can have related causes but require different inspection and acceptance decisions.

For appliance housings, first identify whether the affected area is cosmetic, structural or both. Color, texture, lighting and viewing distance can change how visible a surface mark is, so define the appearance zone and sample reference before approving a remedy.

What to check when a sink appears

  1. Map the defect: Record its location, cavity, material lot, process condition and whether it appears on every shot or only intermittently.
  2. Review the geometry: Look for local thick sections and features that intersect a visible wall. Consider whether a design change can reduce the thickness transition without compromising strength or assembly.
  3. Check the material and gate path: Confirm the resin grade and review whether the gate and runner allow the relevant section to receive packing before the flow path freezes.
  4. Review packing and cooling evidence: Compare the approved process record with measured parts. Packing profile, gate freeze, cooling and material conditions can all affect the result; do not apply a generic pressure or time value.
  5. Validate a change: Change one controlled factor or run an agreed study, then measure the same areas and confirm that the adjustment did not create flash, stress, longer cycle time or another defect.

Autodesk’s troubleshooting guidance identifies thick sections, ribs and bosses, early gate freeze, insufficient packing and cooling as factors to investigate. It also cautions that one remedy can create other problems, so any design or process change needs to be checked against the full mold specification and the actual part.

Agree on acceptance before production

Mark cosmetic surfaces and critical dimensions on the drawing. Define the lighting and viewing conditions for appearance checks, the measurement method for dimensions, and the sample quantity across cavities. Record the approved resin, process window and sample reference so that later production can be compared against the same basis.

For the broader relationship between shrinkage and part distortion, see injection molding shrinkage and warpage. For design inputs, see 注塑成型設計基礎. See the technical reference: Autodesk troubleshooting for sink marks and voids.